【摘要】 BiOBr samples were synthesized by one-step solvothermal method. When the molar ratio of Bi:KBr was 1:2, the synthesized BiOBr had regular morphology, good crystallinity, small band gap, low recombination probability of photogenerated electron-hole, a...